Concrete sealer removal on outdoor pavers at a Kendall home: about 1,500 square feet of concrete slabs set in turf. The pavers had been sealed more than once, with different products, and the layers never bonded. This is part of our concrete restoration work. Here is what we found, what we did, and how it was finished.

Front slab untreated, back slab after the old sealers came off
The Job at a Glance
Kendall | Outdoor concrete pavers | Sealer removal and resealing
STEP 1 OF 3
What We Found
The pavers had been sealed with a combination of different sealers, one on top of another. Different products do not always bond to the concrete or to each other, and these never did. Rolling one more coat over them would only have added another layer with nothing solid to hold onto. The old sealers had to come off first.
STEP 2 OF 3
What We Did
We did a sample area first, so the owner could see the result on their own concrete before we did the whole job. Then every paver was ground with metal diamonds on a planetary floor grinder with a dust shroud and vacuum, with a hand grinder along the edges. Metal diamonds only. The goal was to take the old sealers off and open the pores of the concrete so a new sealer could soak in and bond.

The ground slab next to one still carrying the old sealers
STEP 3 OF 3
How It Was Finished
With the old sealers gone and the pores open, we rolled on StoneTech BulletProof, a water-based penetrating sealer, slab by slab, and let it dry. A penetrating sealer soaks into the concrete instead of sitting on top as a film, and because it went onto bare, open concrete instead of over old layers, it has something to bond to.
Watch the Job | 20 seconds
The grinder taking the old sealers off, then a finished slab next to an untreated one.
Concrete Sealer Removal: Questions People Ask Us
Can a failed sealer be removed from concrete pavers?
Yes. On this Kendall job we ground the old sealers off with metal diamonds on a planetary grinder, then resealed the bare concrete.
Why didn't the old sealer hold?
Different sealers had been put down on top of each other, and they never bonded to the concrete or to each other. Another coat on top would not have fixed that.
Why grind instead of just applying a new sealer?
A new sealer needs bare, open concrete to soak into. Grinding takes the old layers off and opens the pores so the new sealer can bond.
Why do a sample area first?
So you can see the result on your own concrete before we do the whole area.
What sealer did you use?
StoneTech BulletProof, a water-based penetrating sealer. It soaks into the open concrete instead of forming a film on top.
What does it cost?
Every job starts with a $250 assessment, and that $250 is credited in full toward your service.
Sealer Peeling or Patchy on Your Concrete in Kendall?
Text a photo of your concrete to 305-741-9729. Every job begins with a $250 assessment, credited in full toward your service.
More from us: concrete restoration in Miami, tile and grout cleaning in Kendall, and our Google reviews.
Veteran-Owned | 25+ Years | 185+ Five-Star Reviews